ER309L |
主要用于焊接20Cr-14Ni钢 |
C:0.024% Mn:1.65% Si:0.42% Ni:14.33% Cr:20.10% |
拉伸强度Mpa 1200 |
0.08-4.5 |
100/270/300 |
MIG:0.8-1.6 TIG:1.0-4.5 |
|
|
ER309L |
主要用于焊接20Cr-14Ni钢 |
C:0.024% Mn:1.65% Si:0.42% Ni:14.33% Cr:20.10% |
拉伸强度Mpa 1200 |
0.08-4.5 |
100/270/300 |
MIG:0.8-1.6 TIG:1.0-4.5 |