Trade- |
Equivalent to China Standard |
Characteristics & application |
D 667 |
EDZCr-B-15 |
HRc≥48. Resistance to wear, gas corrosion and oxidation. Hardfacing of blast furnace hopper and cracker part. |
D 802 |
EDCoCr-A-03 |
HRc38-47. Resistance to heat, wear and corrosion. Hardfacing of high temperature part such as the edge of thermo-cutter. |
D 812 |
EDCoCr-B-03 |
HRc45-50. Resistance to heat, wear and corrosion. Hardfacing of high temperature part such as internal-combustion engine valve. |
D 822 |
|
HRc≥53. Resistance to Wear and heat, bad shock resistance. Hardfacing of rotating blade wheel of boiler. |
D 832 |
EDCoCr-C-03 |
HRc≥50. Wear and heat resistance. Hardfacing of high temperature part such as hot-rolling guided way. |