Grade :
|
SUS201 弹簧用不锈钢带
|
|
|
|
|
|
|
Number:
|
X12CrMnNiN17-7-5
|
|
|
|
|
|
|
Classification:
|
奥氏体不锈钢-特殊等级
|
|
|
|
|
|
|
Density:
|
7.8 g/cm ³
|
|
|
|
|
|
|
Standard:
|
|
|
|
|
|
|
|
EN 10088-2:2005不锈钢。通用耐腐蚀钢片/板和带材交货技术条件
|
|
|
|
|
|
|
EN 10088-3:2005不锈钢。一般用途耐腐蚀钢的半成品、棒材、线材、型材和光亮产品的交货技术条件
|
|
|
|
|
|
|
EN 10151:2003弹簧用不锈钢带。技术交付条件
|
|
|
|
|
|
|
EN 10088-1:2005不锈钢。不锈钢清单
|
|
|
|
|
|
|
EN 10088-5:2009不锈钢。建筑用耐腐蚀钢棒材、棒材、线材、型材和光亮产品的交货技术条件
|
|
|
|
|
|
|
EN 10088-4:2009不锈钢。建筑用耐腐蚀钢片/板和带材交货技术条件
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Equivalent grades:
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Chemical composition % of steel X12CrMnNiN17-7-5 (SUS201 ): EN 10088-2-2005
|
|
|
|
|
|
|
|
未经买方同意,不得故意将本表中未列出的元素添加到钢材中,除非对铸件进行精加工
|
|
|
|
|
|
|
|
C
|
Si
|
Mn
|
Ni
|
P
|
S
|
Cr
|
N
|
max 0.15
|
max 1
|
5.5 - 7.5
|
3.5 - 5.5
|
max 0.045
|
max 0.015
|
16 - 18
|
0.05 - 0.25
|
|
|
|
|
|
|
|
|
Mechanical properties of steel X12CrMnNiN17-7-5 (SUS201 )
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Rm - Tensile strength (MPa) (+A)
|
750-950
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Rp0.2 0.2% proof strength (MPa) (+A)
|
230-350
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
KV - Impact energy (J) longitud.,
|
+20°
|
|
|
|
|
|
|
100
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
KV - Impact energy (J) transverse,
|
+20°
|
|
|
|
|
|
|
60
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
A - Min. elongation at fracture (%) (+A)
|
40-45
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Brinell hardness (HB): (+A)
|
260
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|